CD STUDS
FLANGED NO THREAD CDFNT
D | FD | MIN L |
---|---|---|
3/32 | .143 | .250 |
.115 | .171 | .250 |
1/8 | .156 | .250 |
.141 | .195 | .250 |
5/32 | .221 | .250 |
.161 | .221 | .250 |
3/16 | .221 | .250 |
.215 | .281 | .312 |
1/4 | .281 | .312 |
.273 | .343 | .312 |
5/16 | .343 | .500 |
![]() MATERIAL |
LOW CARBON STEEL | |
C - 0.23% Max | P - 0.04% Max | |
Mn - 0.90% Max | S - 0.05% Max | |
![]() MECHANICAL PROPERTIES |
Tensile: | 60,000 psi (min) |
Yield: | 50,000 psi (min) | |
Elongation: | 20% (in 2 inches) |
![]() PLATING & ANNEALING |
Copper plating is standard. |
Other plating is available. | |
Studs are annealed where required. |
![]() MATERIAL |
STAINLESS STEEL | |
AISI Grade: 302/304/305 Standard | ||
Other grades are available. | ||
![]() MECHANICAL PROPERTIES |
Tensile: | 85,000 psi (min) |
Yield: | 40,000 psi (min) |
![]() PLATING & ANNEALING |
Studs are annealed where required. |
![]() MATERIAL |
ALUMINUM | |
Alloy: 1100 & 5000 Series | ||
Other alloys are available. |
![]() MECHANICAL PROPERTIES |
Tensile: | 42,000 psi (min) 5000 Series |
Yield: | 30,000 psi (min) 5000 Series |
![]() MATERIAL |
BRASS | |
Alloy (Lead Free) 70-30 is standard. | ||
Other alloys are available. |
![]() MECHANICAL PROPERTIES |
Tensile: | 70,000 psi (min) |
Yield: | 50,000 psi (min) |